Mechanical behavior of iron aluminides: A comparison of nanoindentation, compression and bending of micropillars

  • Mohammad Zamanzade*
  • , Jorge Rafael Velayarce
  • , Oscar Torrents Abad
  • , Christian Motz
  • , Afrooz Barnoush
  • *Corresponding author for this work
  • Saarland University
  • Leibniz-Institute for New Materials
  • Norwegian University of Science and Technology

Research output: Contribution to journalArticlepeer-review

Abstract

Various local testing methods, namely, nanoindentation, compression and bending tests of micropillars were used to better understand the influence of ternary Cr atoms on the extrinsic and intrinsic mechanical properties of Fe3Al intermetallics with the D03 super lattice.Using such local techniques enables us to quantify the influence of Cr on the enhancement of the YoungD's modulus. Furthermore, the effect of Cr on the yield stress, strain hardening and appearance of slip traces was studied based on the stress-strain curves and secondary electron micrographs of the bended and compressed pillars.

Original languageEnglish
Pages (from-to)370-376
Number of pages7
JournalMaterials Science and Engineering: A
Volume652
DOIs
Publication statusPublished - 15 Jan 2016
Externally publishedYes

Keywords

  • Crystal plasticity
  • Dislocations
  • Electron microscopy
  • Intermetallics
  • Micromechanics
  • Nanoindentation