In situ electrochemical nanoindentation of FeAl (100) single crystal: Hydrogen effect on dislocation nucleation
- Afrooz Barnoush*
- , Christian Bies
- , Horst Vehoff
*Corresponding author for this work
- Saarland University
Research output: Contribution to journal › Article › peer-review