TY - JOUR
T1 - Author Correction
T2 - Enhanced hydrogen embrittlement resistance of directed energy deposition 316 L by post-manufacturing heat treatment (npj Materials Degradation, (2025), 9, 1, (62), 10.1038/s41529-025-00590-x)
AU - Liu, Qingyang
AU - Yan, Yan
AU - Iqbal, Muhammad Zeeshan
AU - Tariq, Mohammad
AU - Barnoush, Afrooz
AU - Aissa, Brahim
AU - Farhat, Hanan
N1 - Publisher Copyright:
© The Author(s) 2025.
PY - 2025/12
Y1 - 2025/12
N2 - Correction to: npj Materials Degradationhttps://doi.org/10.1038/s41529-025-00590-x, published online 27 May 2025 In this article the author order was incorrectly given as: Qingyang Liu *, Yan Yan, Muhammad Zeeshan Iqbal, Mohammad Tariq, Afrooz Barnoush, Hanan Farhat & Brahim Aissa* and should have read: ‘Qingyang Liu*, Yan Yan, Muhammad Zeeshan Iqbal, Mohammad Tariq, Afrooz Barnoush, Brahim Aissa* and Hanan Farhat. The original article has been corrected.
AB - Correction to: npj Materials Degradationhttps://doi.org/10.1038/s41529-025-00590-x, published online 27 May 2025 In this article the author order was incorrectly given as: Qingyang Liu *, Yan Yan, Muhammad Zeeshan Iqbal, Mohammad Tariq, Afrooz Barnoush, Hanan Farhat & Brahim Aissa* and should have read: ‘Qingyang Liu*, Yan Yan, Muhammad Zeeshan Iqbal, Mohammad Tariq, Afrooz Barnoush, Brahim Aissa* and Hanan Farhat. The original article has been corrected.
UR - https://www.scopus.com/pages/publications/105019755263
U2 - 10.1038/s41529-025-00690-8
DO - 10.1038/s41529-025-00690-8
M3 - Comment/debate
AN - SCOPUS:105019755263
SN - 2397-2106
VL - 9
JO - npj Materials Degradation
JF - npj Materials Degradation
IS - 1
M1 - 124